1.7131
16MnCr5 | |||||||||
L% | C | SI | Mn | Cr | Ni | Mo | W | V | S |
1.7131 | 0.16 | 0.25 | 1.15 | 0.95 | <0,035 |
Material specification
"Surface-hardened steel for parts with good wear resistance requiring
core tensile strength of 800-1100 N/mm~2"
Application
Piston bolts, camshafts, levers and other vehicle and mechanical
engineering components.
Delivery status: annealed 260HB Max.
Heat treatment
nitrocarburizing