1.2367
X38CrMoV5-3 | |||||||||
L% | C | SI | Mn | Cr | Ni | Mo | W | V | S |
1.2367 | 0.38 | 5.00 | 3.00 | 0.50 |
Material specification
"Hot steel
Depending on the application of EFS and ESR, thermally worked tool
steels have good high temperature wear resistance, high hardness
and temper strength."
Application
Large die casting tools, high temperature and high strength tools,
forging die, mandrel, extrusion die.
Delivery state: annealing state: 229HB Max. Optimum hardness: HRC48-52
Heat treatment